I-Waspaloy, imvula ye-Waspaloy yenza lukhuni i-deformation superalloy

Imininingwane Yomkhiqizo

I-Waspaloy, imvula ye-Waspaloy yenza lukhuni ukuguquguquka kwe-superalloy,
Ipuleti le-waspaloy, Indandatho ye-Waspaloy, Induku ye-Waspaloy,

Amagama Okuhweba Ajwayelekile: Waspaloy, GH4738, UNS N07001,W.Nr.2.4654.

I-Waspaloy iyi-superalloy eqinile yesisekelo se-nickel yobudala enamandla aphezulu okushisa nokumelana nokugqwala okuhle, ikakhulukazi i-oxidation, emazingeni okushisa afinyelela ku-1200°F (650°C) ukuze kusetshenziswe izinhlelo ezishintshayo ezibalulekile, futhi kufika ku-1600°F (870°C. ) kwezinye, izinhlelo zokusebenza ezingafuneki kangako.Amandla okushisa aphezulu engxubevange atholakala ezintweni eziqinisa isixazululo esiqinile, i-molybdenum, i-cobalt ne-chromium, kanye nezinto zayo eziqinisa iminyaka yobudala, i-aluminium ne-titanium.Amandla ayo nokuzinza kwawo kuphakeme kunalawo ngokuvamile atholakala ku-alloy 718.

 

I-Waspaloy Chemical Composition

C

S

P

Si

Mn

Ti

Ni

Co

Cr

Fe

Zr

Cu

B

Al

Mo

0.02 0.10

≤ 0.015

≤ 0.015

≤ 0.15

≤ 0.10

2.75 3.25

U-Bal

12.0 15.0

18.0 21.0

≤ 2.0

0.02 0.08

≤ 0.10

0.003 0.01

1.2 1.6

3.5 5.0

I-Waspaloy Physical Properties

Ukuminyana (g/cm3 )

0.296

Iphoyinti lokuncibilika (℃)

2425-2475

I-Emperature (℃)

204

537

648

760

871

982

I-coefficient yokwandisa ukushisa
(ku/ku°F x 10E-6)

7.0

7.8

8.1

8.4

8.9

9.7

I-Thermal conductivity
(Btu • ft/ft2 • ihora • °F)

7.3

10.4

11.6

12.7

13.9

-

I-Elastic modulus (MPax 10E3)

206

186

179

165

158

144

I-Waspaloy Alloy Typical Mechanical Properties

 

Isimo

Amandla okuqina/MPa

Izinga lokushisa lokusebenza

Ukulungiswa kwesixazululo

800-1000

550ºC

Isixazululo+ukuguga

1300-1500

Anealing

1300-1600

Intwasahlobo eshisayo

1300-1500

¤(Ukusebenza okuqinile kwezinga lokushisa eliphezulu, ukuhlolwa kweshidi lokwelapha ukushisa)

Amazinga we-Waspaloy kanye nokucaciswa

 

Ibha/Induku/Ucingo/Ukufoja I-Strip/Ikhoyili Ishidi/Ipuleti
ASTM B 637, ISO 9723, ISO 9724, SAE AMS 5704, SAE AMS 5706,
SAE AMS 5707, SAE AMS 5708, SAE AMS 5709, SAE AMS 5828,
I-SAE AMS 5544

Imikhiqizo Etholakalayo ye-Waspaloy ku-Sekonic Metals

Ibha ye-Inconel 718, ibha ye-inconel 625

I-Waspaloy Bars & Rods

Amabha ayindilinga/Amabha ayisicaba/amabha e-Hex, Usayizi Kusukela ku-8.0mm-320mm, Isetshenziselwa amabhawodi, izinsimbi nezinye izingxenye eziyisipele

i-welding wire kanye ne-spring wire

Waspaloy Wire

Nikeza ngentambo yokushisela kanye ne-spring wire ngendlela yekhoyili futhi usike ubude.

Ishidi Nepuleti

Ishidi le-waspaloy & plate

Ububanzi bufika ku-1500mm nobude bufika ku-6000mm, Ubukhulu busuka ku-0.1mm kuye ku-100mm.

Ukushesha nokunye Ukufaka

I-Waspaloy Fasteners

Izinto zokwakha ze-Waspaloy ezinhlotsheni zama-Bolts, izikulufu, ama-flanges nezinye izinto ezisheshayo, ngokusho kwamakhasimende.

inconel strip, invar stirp, kovar stirp

I-Waspaloy strip & coil

Isimo esithambile nesimo esiqinile esinendawo ekhanyayo engu-AB, ububanzi bufika ku-1000mm

Kungani Waspaloy?

 I-alloy ekhethekile esekelwe ku-nickel eqina ngeminyaka, amandla aphezulu asebenza kahle ku-1400-1600°F.Ukumelana kahle ne-oxidation esetshenziswa injini ye-turbine yegesi ku-1400-1600 ° F emkhathini.Ngo-1150-1150 ° F, amandla okuqhekeka kwe-Waspaloy aphakeme kunama-718.

Esikalini sika-0-1350 ° F, amandla okushisa ashisayo isikhathi esifushane mabi kakhulu kune-718 alloy

Inkambu yesicelo se-Waspaloy:

I-Waspaloy isetshenziselwa izingxenye zenjini yegesi edinga amandla amakhulu nokumelana nokugqwala emazingeni okushisa aphezulu okusebenza.Izicelo zamanje nezingase zibe khona zihlanganisa ama-compressor nama-rotor disc, ama-shafts, ama-spacers, ama-seal, izindandatho nama-casings, izixhumi nezinye izinhlobo zehardware yenjini, ama-airframe assemblies. kanye nezinhlelo zemicibisholo.

 

I-Waspaloy iyi-superalloy ekhubazekile eqiniswe yimvula, izinga lokushisa elisebenzayo alidluli ku-815 ℃. Ingxubevange inamandla okukhiqiza aphezulu nokumelana nokukhathala ku-760 ℃ ~ 870 ℃, kanye ne-oxidation ephezulu nokugqwala ku-870 ℃, elungele ukukhiqiza amadiski e-WO. , ama-blade asebenzayo, ama-fasteners okushisa aphezulu, amasilinda omlilo, ama-shafts kanye namacala e-WO turbine.Imikhiqizo eyinhloko umugqa ogoqiwe obandayo kanye neshidi eligoqiwe elishisayo, ipayipi, i-strip, intambo, i-forging ne-bolt fasteners, njll.
Uhlobo oluhambelanayo: W.nr 2.4654, UNS N07001, AWS 170
Izinga elisebenzayo :AMS 5544 AMS 5708 AMS 5828