Kuyi-aI-Nickel-Iron, i-alloy enwebekayo ephansi equkethe u-36% we-Nickel enebhalansi ye-Iron.Igcina ubukhulu obucishe bulingane phakathi kobubanzi bamazinga okushisa avamile asemoyeni futhi ine-coefficient ephansi yokunwetshwa ukusuka emazingeni okushisa e-cryogenic ukuya cishe ku-+500°C.I-Nilo 36 nayo igcina amandla amahle kanye nokuqina emazingeni okushisa e-cryogenic.Izicelo zihlanganisa izindinganiso zobude, izinduku ze-thermostat, izingxenye ze-laser namathangi namapayipi okugcina nokuthuthwa kwamagesi anoketshezi.
Ibanga Elihlobene:
Ibanga | Russia | USA | France | EJalimane | E-UK |
4j32 | 32НКД 32НК-ВИ | I-Super-Invar I-Super Nilvar | I-Invar Isikhulu | - | - |
4j36 | 36N 36Н-ВИ | I-Invar/Nilvar Unipsan36 | I-Invar Standard I-Fe-Ni36 | I-Vacodil36 Nilos36 | I-Invar/Nilo36 36 Ni |
4j38 | - | 38NiFM Simonds38-7FM | - | - | - |
C | Ni | Si | Mn | P | S | Fe |
≤0.05 | 35.0-37.0 | ≤0.3 | 0.2-0.6 | ≤0.02 | ≤0.02 | ibhalansi |
Ukuminyana(g/cm3) | I-Meltingtemperature(℃) | Umthamo wokushisa othize/J/(kg•℃)(20~100℃) | Ukumelana nogesi(μΩ·m) | I-Thermalconductivity/W/(m•℃) | Iphoyinti le-Curie(℃) |
8.10 | 1430-1450 | 515 | 0.78 | 11 | 230 |
isimo | σb/MPa | σ0.2/MPa | δ/% |
ukwehlisa | 450 | 274 | 35 |
Ukuqokwa kwe-alloy | I-avareji yokwandisa i-thermal coefficient/(10-6/ ℃) | |||||
20-50 ℃ | 20-100 ℃ | 20-200 ℃ | 20-300 ℃ | 20-400 ℃ | 20-500 ℃ | |
4j36 | 0.6 | 0.8 | 2.0 | 5.1 | 8.0 | 10.0 |
1) I-coefficient yokwandisa okushisayo ephansi kakhulu phakathi kuka-250 ℃ ~ + 200 ℃.
2) Ipulasitiki enhle kakhulu nokuqina
Invar 36 Inkambu yohlelo lokusebenza:
● Ukukhiqizwa kwegesi ye-petroleum ewuketshezi, ukugcinwa nokuthutha
● Krurula isixhumi phakathi kwensimbi nezinye izinto
● Insimbi ephindwe kabili nokulawula izinga lokushisa kwensimbi ephindwe kabili
● Uhlaka lohlobo lwefilimu
● Imaski yethunzi
● Umdwebo wezingxenye ze-CRP zemboni yezokundiza ziyafa
● Uhlaka lweyunithi yokulawula yesathelayithi ne-missile engaphansi kuka-200 ℃
● Ilensi yokulawula i-electromagnetic lens kushubhu ye-vacuum esiza