I-Hastelloy X, i-Superalloy, i-precision alloy, i-monel alloy nickel strip, i-nickel foil,,
Hastelloy X forgings, I-Hastelloy x Plate, Hastelloy x Rod, I-Hastelloy X strip, I-Hastelloy X tube,
I-Hastelloy X iwuhlobo lwe-nickel base superalloy enokuqukethwe kwensimbi ephezulu, eqiniswa kakhulu isixazululo esiqinile se-chromium ne-molybdenum.Ine-anti-metallization enhle nokusebenza kokugqwala, ukukhuthazela okuphakathi namandla okukhasa ngaphansi kuka-900 ℃, ukwakheka okuhle okubandayo nokushisayo kanye nokusebenza kokushisela.
Isetshenziswa ekwenzeni izingxenye zegumbi lomlilo we-aero-injini nezinye izingxenye zokushisa okuphezulu, ngaphansi kuka-900 ℃ isikhathi eside, izinga lokushisa elisebenza isikhathi esifushane lifika ku-1080 ℃.
I-Hastelloy X Chemical Composition
| Ingxubevange | C | Cr | Ni | Fe | Mo | W | Al | B | Co | Si | Mn | P | S |
| Hastelloy X | 0.05~0.15 | 20.5~23.5 | ibhalansi | 17.0~20.0 | 8.0~10.0 | 0.2~1.0 | ≤0.1 | ≤0.005 | 0.5~2.5 | ≤1.0 | ≤1.0 | ≤0.015 | ≤0.01 |
I-Hastelloy X Izakhiwo Zomzimba
| Ukuminyana | 8.3 g/cm³ |
| Iphoyinti lokuncibilika | 1260-1355 ℃ |
I-Hastelloy X Mechanical Properties
| Isimo | Amandla aqinile Rm N/mm² | Amandla esivuno I-Rp 0. 2N/mm² | Ukwelula Njengo-% | Ukuqina kweBrinell HB |
| Ukwelashwa kwesixazululo | 690 | 275 | 30 | > 241 |
| Ibha/Induku | Intambo | I-Strip/Ikhoyili | Ishidi/Ipuleti | Ipayipi/Ipayipi | Ukuqamba |
| I-ASTM B572ASME SB572AMS 5754 | I-AMS 5798 | I-ASTM B435ASME SB435AMS 5536 | I-ASTM B662,ASME SB662 I-ASTM B619,ASME SB619 I-ASTM B626 ,ASME SB626AMS 5587 | I-AMS 5754 | |

Amabha ayindilinga/Amabha ayisicaba/amabha e-Hex, Usayizi Kusukela ku-8.0mm-320mm, Isetshenziselwa amabhawodi, izinsimbi nezinye izingxenye eziyisipele

Nikeza ngentambo yokushisela kanye ne-spring wire ngendlela yekhoyili futhi usike ubude.

Ububanzi bufika ku-1500mm nobude bufika ku-6000mm, Ubukhulu busuka ku-0.1mm kuye ku-100mm.
Usayizi wamazinga kanye nobukhulu obungokwezifiso kungakhiqizwa yithi ngokubekezelelana okuncane

Isimo esithambile nesimo esiqinile esinendawo ekhanyayo engu-AB, ububanzi bufika ku-1000mm

Izinto zokwakha ze-Hastelloy X ezinhlotsheni zama-Bolts, izikulufu, ama-flanges nezinye izinto ezisheshayo, ngokuya ngemininingwane yamakhasimende.
1. Ukumelana ne-oxidation okuhle kakhulu ekushiseni okuphezulu(>1200℃)).
2. Amandla amahle ezinga lokushisa eliphezulu.
3. Ukwakheka okuhle nokushisela.
4. Ukumelana kahle nokuqhekeka kokugqwala kwengcindezi.
Ngenxa yokumelana nokugqwala kwayo ezindaweni ezishisayo ezishisayo kanye namandla aphezulu okushisa aphezulu, i-HastelLoyx isetshenziswe kabanzi ezindaweni ezihlukahlukene zokushisa okuphezulu.
Izinkambu ezijwayelekile zohlelo lokusebenza:
•Izinjini zezitimu zezimboni nezokundiza (amakamelo omlilo, izilungisi, izikepisi zesakhiwo)
•Izingxenye zesithando somlilo sezimboni, ama-roller asekelayo, ama-grate, amaribhoni namashubhu erediyetha
•Amashubhu e-Spiral ezithandweni ze-petrochemical
•Igesi lokushisa eliphezulu lipholisa i-nuclear reactor
I-Sekonic metal Technology Co., Ltd. ipuleti lokunikezela, i-strip, insimbi eyindilinga, ipayipi, intambo, ama-forgings, i-ingot, i-flange, i-tee, indololwane, ukucaciswa okuphelele namamodeli
impahla
Okujwayelekile: I-alloy steel F5 ne-410; Insimbi engagqwali 304, 304L, 316, 316L, 321 kanye ne-347.
Okungajwayelekile: ingxubevange ye-nickel ephezulu (inconel 718, inconel 625, inconel 825, inconel 925, alloy 20,GH3030, nimoni 80A), izinga lokushisa eliphezulu lensimbi yealloy (haines 25,25, haines 188, njll.) namanye amamaki ensimbi engagqwali.
Ukuqinisekiswa kwekhwalithi, intengo ethengekayo, isikhathi esifushane sokulethwa, hlinzeka ngewaranti yokuqala yasefekthri, uma udinga ukwamukela ukushayela ucingo lokubonisana nomakhalekhukhwini/whatsapp: 0086-15921454807