Le alloy ezithambile kazibuthe ehlanganisa 49% Nickel, ibhalansi Iron esetshenziswa lapho high permeability kwasekuqaleni.ukufinyeleleka okuphezulu, kanye nokulahlekelwa okuyisisekelo okuphansi kuyadingeka
Izinhlelo zokusebenza:
• I-electro-magnetic shielding • Ukukhanyisa okukhethekile kwe-transformer• Amanxeba amanxeba e-Toroidal tape • Ama-motor laminations ekhwalithi ephezulu • Izinjini zokunyathela
Ibanga | E-UK | EJANPAN | USA | Russia | Okujwayelekile |
I-Supermalloy (1J50) | I-Mumetal | PCS | Hy-Ra49 | 50H | I-ASTM A753-78 I-GBn 198-1988 |
I-alloy50(1J50)Ukwakheka Kwamakhemikhali
Ibanga | Ukwakhiwa Kwekhemikhali (%) | |||||||
C | P | S | Cu | Mn | Si | Ni | Fe | |
I-Supermalloy1j50 | ≤ | |||||||
0.03 | 0.020 | 0.020 | 0.20 | 0.30~0.60 | 0.15~0.30 | 49.5~50.5 | Ibhalansi |
I-alloy50(1J50)Impahla Engokomzimba
Ibanga | Ukungazweli (μΩ•m) | Ukuminyana (g/cm3) | Iphoyinti leCurie °C | I-saturation magnetostriction constant (× 10-2) | Amandla Okuqina/MPa | Amandla e-Yelid/MPa | ||
I-Supermalloy 1j50 | ||||||||
0.45 | 8.2 | 500 | 25 | 450 | 150 |
I-lloy50(1J50)Isilinganiso Sokunwetshwa Komugqa
Ibanga | I-Coefficient of Linear Expansion at Different Temperaturel(x 10-6/K) | ||||||||
20℃100℃ | 20℃ 200℃ | 20℃ 300℃ | 20℃400℃ | 20℃ 500℃ | 20℃ 600℃ | 20℃ 700℃ | 20℃ 800℃ | 20℃ 900℃ | |
Ingxubevange 50 1j50 | 8.9 | 9.27 | 9.2 | 9.2 | 9.4 | -- | -- | -- | -- |
I-Mumetal Shielding Potential
I-Permalloy inokufinyeleleka okuphezulu kakhulu namandla okuphoqelela okuzenzela ayenza ibe into efanelekile yokusebenza kokuvikela.Ukuze kuzuzwe izakhiwo ezifiselekayo zokuvikela, i-HyMu 80 ixhunywe kufika ku-1900oF noma ku-1040oC kulandela ukwakheka kwezinqubo.I-Annealing emazingeni okushisa aphakeme kuthuthukisa ukufinyeleleka kanye nezakhiwo zokuvikela.